Sandpaper is the cheapest thing in the workshop and the one that decides whether a finish looks professional. The grit number is only part of the specification: the backing, the abrasive grain and the way the sheet is held all change how it cuts, how long it lasts and whether it clogs. This guide covers the sheets, discs and rolls we stock and how to build a grit sequence that actually reaches a finish.
Reading the specification
- Grit (P-grade). The lower the number, the coarser the cut. P40 removes material fast and leaves deep scratches; P2000 refines a surface and removes almost nothing.
- Grain. Aluminium oxide suits wood and steel, silicon carbide suits paint, filler, stone and wet work, and ceramic grain cuts faster and lasts longer on hard material.
- Backing. Paper backing is for fine work and clogs when wet. Cloth backing survives edges and heat. Film backing stays flat and is what keeps a precision sheet dimensionally stable.
- Open or closed coat. An open coat leaves gaps between grains so dust escapes, which is what keeps a sheet from clogging on paint and softwood.
Matching the abrasive to the job
| Job | Grain and backing | Note |
|---|---|---|
| Stripping paint and varnish | Silicon carbide, open coat | Clogs fast, so change sheets often |
| Shaping bare timber | Aluminium oxide, paper or cloth | Start coarse enough to remove the damage |
| Flatting between coats | Fine silicon carbide, waterproof | Use wet to stop the paper loading up |
| Metal and rust | Aluminium oxide or ceramic on cloth | Edges shred paper backing |
| Filler and primer | Silicon carbide, P180 to P400 | Filler clogs coarse paper immediately |
Discs for machine sanding
Hook-and-loop sanding discs in 125 mm from 40 to 2000 grit with six or eight holes are the workhorse for random orbital sanders, and the hole pattern is not cosmetic: it lets the dust extraction pull through the disc, which is what stops the surface loading and keeps the abrasive cutting. Hook-and-loop discs with a velour backing for wood hold their position on the pad and resist tearing at the edge. Buy the grits you actually use in bulk and the rest in small packs, because a worn disc polishes the surface instead of cutting it.
Sheets, rolls and precision work
Self-adhesive precision sandpaper in 279 to 350 mm, waterproof sticks to a flat block or a machine platen, which is what keeps a face dead flat rather than rounded. Precision finishing sandpaper in carbon silicon for furniture and paint work covers the fine end of the sequence, and waterproof silicon carbide sandpaper is the sheet that keeps working when it is wet, which is how you flat a lacquer without clogging the paper. For high walls and ceilings, a swivel sanding head on a two to four metre extension pole reaches the surface without a ladder, and the swivel joint is what keeps the head flat against the wall as you move.
Building a grit sequence
The rule is simple and mostly ignored: never skip more than one grade, and never move to a finer grit until the scratches from the previous one have gone. A typical sequence on bare timber runs P80 to remove damage, P120, P180, then P240 before a finish, with P320 or finer only where the finish demands it. Skipping from P80 to P240 leaves deep scratches that the fine grit cannot remove, so the surface looks polished and then shows every mark as soon as the first coat goes on.
Why paper stops cutting, and how to fix it
- Loading. The gaps between grains fill with dust or paint. Use an open coat, use extraction, and on paint use a wet sheet.
- Glazing. Heat melts the finish or the resin binder onto the grain. Reduce pressure and speed rather than pressing harder.
- Worn grain. The abrasive has dulled. No amount of pressure will bring it back, so replace the sheet.
- Wrong grain. Aluminium oxide on paint clogs; silicon carbide on steel wears quickly. Match the grain to the material.
Technique and safety
Sanding is a cutting operation, so let the grit cut and keep the pressure light. Pressing hard generates heat, which glazes the paper and burns the surface, and it rounds the edges of a workpiece because the paper deforms over the corner. Use a block or a pad to keep a face flat, work along the grain on timber, and dust off between grits so loose grit from the previous grade does not scratch the new surface. Wear eye protection and a mask: dust from sanding paint, filler and composite material is a genuine respiratory hazard, and old paint may contain materials you do not want to breathe. Where you sand inside, use extraction rather than a fan, because a fan simply moves the dust around the room.
Frequently asked questions
What grit should I start with?
Coarse enough to remove the damage in one pass without creating more work than necessary. P80 is a typical starting point for bare timber, P120 to P180 for a surface that only needs keying.
Can I skip grits?
You can skip one grade if the surface is already fine, but skipping several leaves scratches that the finer grit cannot remove. The time saved is lost when the finish reveals them.
What is the difference between P-grade and CAMI grit?
They are different scales. A P-grade number is not the same as the same CAMI number; P80 is close to CAMI 80 but they diverge as the number rises.
Why does my sandpaper clog with paint?
The coat is closed, the paper is being run too fast, or the paint is not fully cured. Use an open-coat or waterproof sheet and reduce the speed.
Can I use sandpaper wet?
Only waterproof paper with a suitable backing and grain, usually silicon carbide. Ordinary paper backing disintegrates when it gets wet.
Where to start
Browse the full Sandpaper range, or the wider Abrasives category if you also need belts, discs or polishing compounds. Tell us the material, the finish you need and whether you sand by hand or machine, and we will point you at the grain, backing and grit sequence that fit.